MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Epsan Eplamid 66 NC P Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: An unreinforced polyamide 66, externally and internally lubricated for injection molding where fast cycles are required. Eplamid 66 NC P offers all of primary properties of unreinforced polyamide 66.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 1.4 %
@Time 86400 sec
1.4 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.018 cm/cm0.018 in/inParallel; ISO 294-4
 0.019 cm/cm0.019 in/inNormal; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 82.0 MPa11900 psiISO 527-2
Elongation at Break 50 %50 %ISO 527-2
Elongation at Yield 4.2 %4.2 %ISO 527-2
Tensile Modulus 3.20 GPa464 ksiISO 527-2
Flexural Strength 95.0 MPa13800 psiISO 178
Flexural Modulus 2.90 GPa421 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VEN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 261 °C502 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 204 °C399 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °FISO 75-2/A
Flammability, UL94  V-2
@Thickness 0.400 mm
V-2
@Thickness 0.0157 in
EN 60695-11-10
 V-2
@Thickness 0.710 mm
V-2
@Thickness 0.0280 in
EN 60695-11-10
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
EN 60695-11-10
Glow Wire Ignition Temperature  750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
EN 60695-2-13
 900 °C
@Thickness 1.50 mm
1650 °F
@Thickness 0.0591 in
EN 60695-2-13
 960 °C
@Thickness 0.710 mm
1760 °F
@Thickness 0.0280 in
EN 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.710 mm
1760 °F
@Thickness 0.0280 in
EN 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
EN 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPSAN088 / 186402

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.