MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos K38-20-123 Pipe Extrusion Grade Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: K38-20-123 is a black medium density polyethylene resin designed specifically for pipe extrusion and pipe coating. It exhibits excellent long term stress life and environmental stress crack resistance. This material has NSF certification for potable water applications and is recognized by the Plastics Pipe Institute as having a PE 2406 rating. The natural version of this resin is K38-20-138. ASTM D3550 cell classification of this resin is 234343C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccBlack density
 0.949 g/ccASTM D4883
Environmental Stress Crack Resistance 2000 hourCond. B, 10%; ASTM D 1693
 5000 hourCond. C, ASTM D 1693
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ASTM D2240
Tensile Strength, Ultimate 31.03 MPa2 in/min.; ASTM D638
Tensile Strength, Yield 19.31 MPa2 in/min.; ASTM D638
Elongation at Break 800 %2 in/min.; ASTM D638
Flexural Modulus 0.689 GPa
@Strain 2 %
Secant; ASTM D 790
Izod Impact, Notched 5.38 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 120 °CASTM D1525
Brittleness Temperature -75.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil BA53-055 High Density Polyethylene Resin
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
LG Chemical SEETEC PB283 HDPE
Petromont 4102 High Density Polyethylene Resin
Formosa Plastics Formolene® HP6000 Pipe HDPE

PSOLKD / 68220

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.