MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cookson Group STAYDRY® H2-3000 Hydrogen and Moisture Getter  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: Hermetically sealed semiconductor devices containing Gallium Arsenide (GaAs), RF absorbers and utilizing industry gate metallization structures have been shown to leak out hydrogen in ambient as well as environmental conditioning, which will poison and shorten the life of the device. CSPM manufactures and sells the hydrogen getter for the semiconductor industry, specifically designed for these types of devices.

H2-3000 film is a unique getter, which employs an active hydrogen getter and desiccant for water absorption, dispersed in a flexible silicone polymer matrix. The high permeability of the polymer matrix to both hydrogen and moisture assures a rapid uptake of both gases. The getter operates through a reaction, which is irreversible for hydrogen. Therefore, there are no hazardous or problematic side effects, once absorbed gasses are trapped from harming the device.

Properties:

H2-3000 possesses high hydrogen and moisture gettering capacity, while being thermally stable up to 200°C. The material is a film and can therefore be molded or stamped to any desired shape. The excellent physical properties of the polymer allow the getter to remain flexible over the temperature range of –55°C to 150°C. As a result, no spalling or flaking occurs as the getter material removes hydrogen. The composition of the material is designed to maintain a dew point of less than –65°C, while maintaining a hydrogen atmosphere of less than 1 part per million within the device.

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 - 1.50 g/cc
Moisture Absorption at Equilibrium >= 3.5 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 440 µm/m-°C
@Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Monthat 25°C
 
Descriptive Properties
AppearanceBlack film
Getter Activation16 hours at 150°CVacuum oven, <500 micron Hg
Hydrogen Capacity=45 cm3/g
Hydrogen Rate<1 ppmWithin 24 hours
Thermal Stability<1.0% loss

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLASK071 / 56361

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.