MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound 2X98703 Ethylene Tetrafluoroethylene Copolymer (ETFE)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: LNP THERMOCOMP 2X98703 compound is based on Ethylene Tetrafluoroethylene (ETFE) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.73 g/cc1.73 g/ccASTM D792
Density 1.73 g/cc0.0625 lb/in³ASTM D792
Moisture Absorption 0.0100 %0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0100 %0.0100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 88.0 MPa12800 psi5 mm/min; ISO 527
 98.0 MPa14200 psi5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa13800 psi5 mm/min; ISO 527
 101 MPa14600 psi5 mm/min; ASTM D638
Elongation at Break 5.5 %5.5 %5 mm/min; ISO 527
 5.9 %5.9 %5 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %5 mm/min; ISO 527
 5.6 %5.6 %5 mm/min; ASTM D638
Tensile Modulus 11.22 GPa1627 ksi1 mm/min; ISO 527
 14.18 GPa2057 ksi5 mm/min; ASTM D638
Flexural Strength 135 MPa19600 psiyield, 2 mm/min; ISO 178
 143 MPa20700 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 10.44 GPa1514 ksi2 mm/min; ISO 178
 10.6 GPa1540 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 411 J303 ft-lbASTM D256
Izod Impact, Unnotched 4.81 J/cm9.01 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 34.0 kJ/m²16.2 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 88.0 kJ/m²41.9 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 20.0 J14.8 ft-lbASTM D3763
Impact Test 8.00 J5.90 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 239 °C462 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 248 °C
@Thickness 3.20 mm
478 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 187 °C369 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 214 °C
@Thickness 3.20 mm
417 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 300 - 325 °C572 - 617 °F
Zone 3 325 - 340 °C617 - 644 °F
Melt Temperature 315 °C599 °FInjection Molding
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81438 / 289385

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.