MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Silicon Carbide Nitrite Bonded Pressed Thermal Ceramic
Categories: Ceramic; Carbide

Material Notes: Silicon Nitride bond. The silicon nitride bond phase in these refractories is the key to their superior performance in demanding applications. The Morsil™ nitride bonding system allows nitride bonded refractories to out-perform other silicon carbide based refractories using silicate, alumina silica, and silicon oxynitride and beta silicon carbide bond systems. The alpha silicon carbide crystals impart high thermal conductivity and refractoriness, low thermal expansion and outstanding abrasion/erosion resistance.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.62 g/ccASTM 134
Porosity 17 %
Permeability 3.0cc of air/min/in/m2/in WG press
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0400 GPa
@Temperature 20.0 °C
 0.0400 GPa
@Temperature 1350 °C
Compressive Strength <= 137 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.70 µm/m-°C
Specific Heat Capacity 0.280 BTU/lb-°F
@Temperature 1400 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 1477 °C
ASTM C 202
Maximum Service Temperature, Air <= 1700 °Cmax. hot face temp.
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.30 %
CaO 0.20 %
Fe2O3 0.30 %
Other 0.30 %trace
Si3N4 23.4 %
SiC 75 %
SiO2 0.50 %
 
Descriptive Properties
Electrical Characteristicssemi-conductor
Spall Resistance (%)100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Reaction-Bonded, SiSiC
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
CeramTec Rocar® S Silicon Carbide, SSiC
G-11 Fiberglass Epoxy Laminate Sheet

CMORF6230 / 203014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.