MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CRM 18D Cast Iron-Nickel Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: Typical Application: Automotive gas turbines

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  131 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
19000 psi
@Temperature 1500 °F,
Time 1000 hour
 172 MPa
@Temperature 816 °C,
Time 360000 sec
25000 psi
@Temperature 1500 °F,
Time 100 hour
 234 MPa
@Temperature 732 °C,
Time 3.60e+6 sec
34000 psi
@Temperature 1350 °F,
Time 1000 hour
 290 MPa
@Temperature 732 °C,
Time 360000 sec
42000 psi
@Temperature 1350 °F,
Time 100 hour
 372 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
54000 psi
@Temperature 1200 °F,
Time 1000 hour
 434 MPa
@Temperature 649 °C,
Time 360000 sec
63000 psi
@Temperature 1200 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.0030 %0.0030 %
Carbon, C 0.75 %0.75 %
Chromium, Cr 23 %23 %
Cobalt, Co 5.0 %5.0 %
Iron, Fe 57.497 %57.497 %Balance
Manganese, Mn 5.0 %5.0 %
Nickel, Ni 5.0 %5.0 %
Niobium, Nb (Columbium, Cb) 2.0 %2.0 %
Nitrogen, N 0.25 %0.25 %
Silicon, Si 0.50 %0.50 %
Tungsten, W 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-4.5Al-3V-2Mo-2Fe (SP-700)
PSM Industries PM Krupp M-2 Powder Metallurgy Steel Alloy
Nickel Gear Bronze, UNS C91700, Sand Cast
MetalTek MTEK 440A Martensitic Stainless Steel
Kennametal Stellite Nucalloy® 45 (Stoody® 45) Nickel-Chromium-Boron Alloy

NZ97054 / 191452

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.