MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Catalyst Masterbatch CT 0552/09 Polyolefin
Categories: Other Engineering Material; Catalyst/Initiator; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Catalyst Masterbatch CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or steam at high temperature. Catalyst Masterbatch CT 0552/09 contains a processing aid.

Antioxidant; Thermal Aging Resistant

Uses: Connectors; Hose; Potable Water Applications

Processing: Extrusion; Pipe Extrusion

Agency Ratings: DVGW W270; KTW Unspecified Rating

Availability: Asia Pacific; Europe; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.550 g/ccASTM D1895
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Processing PropertiesOriginal ValueComments
Zone 1 150 - 200 °C
Zone 2 150 - 200 °C
Zone 3 150 - 200 °C
Zone 4 150 - 200 °C
Zone 5 150 - 200 °C
Die Temperature 210 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/930 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/325 Polyolefin
Syensqo (Solvay Specialty Polymers) Polidiemme® G/220 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Polidiemme® G/420 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/365 Polyolefin

PSOL8Y6126 / 193047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.