MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Material and Design Solutions MDS Petroz™ 375 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Material & Design Solutions’ (MDS) Petroz™ perfluoroelastomer (FFKM) is a superior choice for sealing in the most challenging environments. Effective at temperatures up to 250°C (482°F), Petroz compounds have a broad chemical resistance in aggressive chemical environments such as H2S, amine-based (high pH) corrosion inhibitors, organic solvents, and strong acids. These compounds also offer a significantly lower compression set compared to competitive products providing longevity and a more effective sealing solution. Petroz FFKM compounds are designed to operate and excel in high temperature, high pressure, and hostile chemical environments. In addition, Petroz 595 has superior rapid gas decompression (RGD) resistance and has demonstrated excellent RGD resistance in laboratory (ISO 23936-2 and NORSOK M-170) testing. Petroz compounds are totally fluorinated and offer the ultimate chemical resistance required in downhole applications as well as in mechanical seals, pumps, and valves in a variety of industries.

Finished Parts: MDS offers Petroz FFKM in the form of molded finished products for critical service applications.

Typical Applications:

  • O-Rings
  • V-Rings
  • Gaskets
  • T-Rings
  • X-Rings
  • Custom molded products

Information provided by Material & Design Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.99 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Tensile Strength at Break 23.0 MPaASTM D412
Elongation at Break 160 %ASTM D412
Flexural Modulus 4.00 MPa
@Strain 50 %
ASTM D412
Compression Set 14 %
@Temperature 200 °C,
Time 252000 sec
ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMDS000 / 318090

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.