MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos J52-08-226 High density polyethylene copolymer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: J52-08-226 is a bimodal high molecular weight high density polyethylene copolymer designed for thin gauge blown film applications where good process ability, high stiffness and excellent strength are required such as: Grocery sacks, T-Shirt bags, Institutional/Industrial Can Liners, Roll Stock, Produce Bags, Heavy Duty Bags and Deli Wrap. J52-08-226 meets the requirements of the U.S. Food and Drug Administration of 21 CFR 177.1520 covering the safe use of articles intended for use in food contact applications. (Specific limitations may apply. Consult the J52-08-226 Regulatory Position statement for more information.)

Film property data based on 0.6 mil film (15 micron) obtained under laboratory conditions at a 4:1 Blow-Up-Ratio (BUR) and stalk height of 7x die diameter.

Information provided by INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D4883
ESCR 100% Igepal® >= 1500 hour>= 1500 hourCondition B, F50; ASTM D1693B
Melt Flow  0.31 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.31 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 34.5 MPa
@Thickness 0.0150 mm
5000 psi
@Thickness 0.000591 in
ASTM D882
Film Tensile Strength at Yield, TD 31.0 MPa
@Thickness 0.0150 mm
4500 psi
@Thickness 0.000591 in
ASTM D882
Elmendorf Tear Strength MD 18 g
@Thickness 0.0150 mm
18 g
@Thickness 0.000591 in
ASTM D1922
Elmendorf Tear Strength TD 180 g
@Thickness 0.0150 mm
180 g
@Thickness 0.000591 in
ASTM D1922
Dart Drop Test 350 g
@Thickness 0.0150 mm
0.772 lb
@Thickness 0.000591 in
F50; ASTM D1709
Film Tensile Strength at Break, MD 69.0 MPa
@Thickness 0.0150 mm
10000 psi
@Thickness 0.000591 in
ASTM D882
Film Tensile Strength at Break, TD 62.0 MPa
@Thickness 0.0150 mm
8990 psi
@Thickness 0.000591 in
ASTM D882
1% Secant Modulus, MD 930 MPa
@Thickness 0.0150 mm
135000 psi
@Thickness 0.000591 in
2% Secant Modulus; ASTM D882
1% Secant Modulus, TD 1035 MPa
@Thickness 0.0150 mm
150100 psi
@Thickness 0.000591 in
2% Secant Modulus; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 124 °C255 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21CFR 177.1520

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOS862 / 291468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.