MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials BETAFORCE™ 2816L Polyurethane Adhesive
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: 2-component polyurethane adhesive with moderate modulus and long working time at room temperature, suitable for structural bonding.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.19 g/cc0.0415 - 0.0430 lb/in³Component A
 1.41 - 1.45 g/cc0.0509 - 0.0524 lb/in³Component B
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 0.0210 GPa3.05 ksiISO 527-1/-2
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 90.0 °C<= 194 °FTemperature stability
Minimum Service Temperature, Air -40.0 °C-40.0 °FTemperature stability
 
Processing PropertiesMetricEnglishComments
Processing Temperature 18.0 - 28.0 °C64.4 - 82.4 °Fdepends strongly on temperature
Tack-Free Time 35.0 - 50.0 min0.583 - 0.833 hour23°C on 30 - 50 cm length adhesive beads
Shelf Life 6.00 Month
@Temperature 5.00 - 25.0 °C
6.00 Month
@Temperature 41.0 - 77.0 °F
at +5°C to + 25°C
 
Descriptive Properties
BasisPolyol and isocyanate
ColorBlackComponent A
 WhiteComponent B
Extrusion Viscosity20 to 35Component A; 2mm, 4bar
 25 to 40Component B; 2mm, 4bar
PolymerAdhesive
Regional AvailabilityEurope
 Near East/Africa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9016x / 290837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.