Grilamd L16 GM is a low-viscosity, non-reinforced PA 12 grade, UV- and heat-stabilized. The modification with a crystallization regulator causes a quick freeze and a fine, crystalline structure. Due to its good flowability, Grilamid L16 GM is especially suitable for thinwalled injection molding applications.Information provided by EMS Grivory. |