MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2248 is a thixotropic, high temperature cure, 100% solids epoxy resin system that provides strong, tough bonds between a wide range of materials (includes metals, glass, ceramics, and many plastics). This adhesive is recommended for bonding applications up to 190°C where good high and low temperature mechanical and electrical properties are required. It is an all liquid system that is easily mixed and handled and applied at room temperature although a final high-temperature cure is REQUIRED for satisfactory bonds. Fully cured TRA- BOND 2248 has excellent impact and thermal shock resistance, low permeability to gases and vapors, and outstanding resistance to water, weather, oxygen and ozone, most petroleum solvents and fuels, mild acids and alkalis, and many other organic and inorganic compounds. This system complies with specification ASTM E-595-90 for NASA outgassing acceptability. An additional post-cure of 2 hours at 125°C is recommended when application temperatures higher than 125°C are anticipated.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccMixed
Water Absorption 0.0010 %After 24 hours
Viscosity 10000 cP
@Temperature 25.0 °C
Mixed (sp #4, 12 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
Tensile Strength, Yield 10500 psi
Elongation at Yield 2.0 %
Adhesive Bond Strength 2600 psiLap shear, alum to alum
Izod Impact, Notched 0.520 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+15 ohm-cm
Dielectric Constant 4.35
@Frequency 1000 Hz
Dielectric Strength 375 V/mil
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 190 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 109 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 100 °C
Pot Life 120 min
 
Descriptive Properties
Color Tan
Heat Distortion Temperature °C148
Mix Ratio, parts by weight100/19.4Resin/Hardener
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Aptek 2120 PMF Low modulus urethane staking compound
Aptek 2100-A7C/B Low modulus urethane staking compound
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound

PTRAC069 / 70997

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.