MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Trivalence Technologies Polymers

(Viewing data as-entered. Click here to return)
Trivalence Technologies TriVET™ 11B (U,R) Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Polybutylene Terephthalate, low flow, general purpose

Typical Applications: Transportation, housing, electrical

Information provided by Trivalence Technologies.

Vendors: Trivalence Technologies offers solution driven Custom Compounding, Distribution and Applied Sciences to the world’s plastic injection and extrusion markets. We pair our leading-edge resins and blends with personal attention to each customer’s needs. We work with you one-on-one at every stage and at every level to make sure you have an exceptional experience every time. Click to view more about the services we offer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.018 - 0.020 in/in
@Thickness 3.20 mm
TVT Internal Test
Melt Flow 10 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ISO 2039
Tensile Strength, Yield 58.0 MPaISO 527
Tensile Modulus 2500 MPaISO 178
Charpy Impact, Notched 3.40 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.0 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 301 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 122 °FISO 75
Vicat Softening Point 364 °FISO 75
Flammability, UL94 HB
@Thickness 1.52 mm
TVT Internal Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 275 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 110 - 130 °C
@Time 10800 - 21600 sec
Moisture Content 0.020 %
 
Descriptive Properties
AvailabilityAsia
 Europe
 Latin America
 North America
CharacteristicLow Flow
ColorAll
FormPellets
Outdoor Suitability (QUV)PassTVT Internal Test, "U" Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRIV9851 / 313743

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.