Product: PLEXIGLAS® Film 0F063 is a very high weather resistant and transparent acrylic film for graphic printings and lamination systems. Due to its excellent performance under weathering and UV light exposure, PLEXIGLAS® Film 0F063 does not present color change or yellowing. Therefore it provides high protection of polymeric substrates from degradation caused by UV radiation. Its very smooth surface leads the film to have a good optical quality surface. Application: PLEXIGLAS® Film 0F063 is suitable as top layer for high UV and weathering protection of different polymeric substrates including ones based on Fiber Reinforced Polyester Resin. PLEXIGLAS® Film 0F063 can be used to be printed on as good quality film decoration and then laminated on different polymeric films or sheets. Laminated decoration films based on PLEXIGLAS® are suitable for a wide range of molding processes such as thermoforming and insert molding. The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm). |