MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -40°C (-40°F). Good mildew/bacteria resistance per ASTM G-21. Skin contact is 'no irritation' per Schwartz and Peck human patch test. No stain per ASTM D925. Good UV resistance per ASTM G53. No tackiness or surface deterioration after 10 min. immersion in 75% naphtha, 25% 1,1,1-trichloroethane, then allowed to dry completely. No tackiness or surface deterioration in antifreeze + water 50/50; windshield washer solution; electrical grease; or in soap + water 50/50. Passes ozone resistance per GM 4486P.

General Poron® information: Poron® foams are supplied in continuous rolls and can easily be fabricated: die-cut, slit, machined, and laminated. Key properties include excellent resistance to compression set, high energy absorption, low outgassing, resistance to temperatures, bondable surface, low hydrolysis, no plasticizers, high internal strength and dimensional stability, and chemical resistance.

Information supplied by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 g/cc±10%; ASTM D3574A
Water Absorption 2.0 %Typical per AMS 3568
Water Absorption at Saturation 19 %Immersion; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8.0ASTM D2240
Hardness, Shore O 12ASTM D2240
Tensile Strength, Ultimate >= 0.276 MPaASTM D3574E
Elongation at Break >= 100 %ASTM D3574E
Compressive Yield Strength 0.0270 - 0.0550 MPaat 25% deflection; 0.2"/min strain rate
Tear Strength >= 0.500 kN/mDie C; ASTM D624
Compression Set <= 2.0 %
@Temperature 23.0 °C
ASTM D1667 test D
 <= 5.0 %
@Temperature 121 °C
Test D after autoclaved 5 hrs.; ASTM D3574J
 <= 10 %
@Temperature 70.0 °C
ASTM D3574 test D
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 ohm-cmASTM D257
Surface Resistance 2.00e+12 ohmASTM D257
Dielectric Constant 1.71K' ("DK"); ASTM D150; relative humidity 50% for 24 hrs.
Dielectric Strength 2.00 kV/mmASTM D149
Dissipation Factor 0.050tan D ("DF"); ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 230 - 310 µm/m-°C
@Temperature 20.0 °C
ASTM C518
Maximum Service Temperature, Air 90.0 °CRecommended continuous use
 121 °CIntermittent
Brittleness Temperature -40.0 °CLow temp embrittlement; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam
Aearo E-A-R Specialty Composites Isodamp® C-1000 Series TPE
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam
GEHR Plastics PVC type I®

PROGPO3 / 66296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.