MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good surface, chemical resistance and high electrical performance.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 98.1 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 156.96 MPaASTM D790
Flexural Modulus 6376.5 MPaASTM D790
Izod Impact, Notched 15.0 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 178 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 270 °C
Mold Temperature 60.0 - 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LIGHTER™ C93 Polyethylene Terephthalate (PET) Resin
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
Celanese Celanex® 2302 GV1/30 PBT, 30% Glass Reinforced
Evonik Vestodur® GF 30 30% Glass Reinforced PBT
Celanese Celanex® 2300 GV3/30 PBT, 30% Glass Reinforced

PEPOLZ027 / 103524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.