MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem STEARIC ACID RG
Categories: Other Engineering Material

Material Notes: Product Description: Stearic Acid (Rubber Grade) is a mixture of fatty acids composed primarily of octadecanoic (stearic), and hexadecanoic (palmitic 50%) acids to a controlled titer (molecular composition) and acid value (presence of unsaturation). It is a light-colored, waxy solid with a characteristic fatty odor. Akrochem’s stearic acid is available in flake form. The flake form is primarily tallow-based. Stearic acid has FDA status under 177.2600 regulations.

Application: Stearic acid is used as a dispersing agent and accelerator activator in rubber compounds. It aids dispersion of pigments and fillers and improves processing since it acts as a stock lubricant and can facilitate mold flow, improve extrusions and aid release. For a higher purity mixture of saturated fatty acids see Akrochem’s Stearic Acid TP (triple pressed).

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 g/cc0.850 g/cc
 
Chemical PropertiesMetricEnglishComments
Acid Value 193 - 214193 - 214[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 70.0 °C158 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 4.04.0
 
Descriptive Properties
Content0.07Miscellaneous Saturated Acids
 0.09Oleic Acid
 0.35Stearic Acid
 0.5Palmitic Acid
Iodine Value<10
Saponification Number195-214 mg KOH/g
Titer>52°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH418 / 315336

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.