MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Crastin® FR1301TC BK350 PBT-I-CD40FR(17)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 39.0 MPa5660 psiISO 527-1/-2
Elongation at Break 1.0 %1.0 %ISO 527-1/-2
Tensile Modulus 7.10 GPa1030 ksiISO 527-1/-2
Flexural Strength 57.0 MPa8270 psiISO 178
Flexural Modulus 8.30 GPa1200 ksiISO 178
Poissons Ratio 0.350.35
Charpy Impact Unnotched 0.790 J/cm²
@Temperature 23.0 °C
3.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.240 J/cm²
@Temperature 23.0 °C
1.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 ohm-cm1.00e+8 ohm-cmtested at 2mm thickness and 10V; IEC 62631-3-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 28.0 µm/m-°C15.6 µin/in-°FISO 11359-1/-2
Thermal Conductivity 10.0 W/m-K69.4 BTU-in/hr-ft²-°FIn Plane; ASTM E 1461
 1.00 W/m-K
@Thickness 0.300 mm
6.94 BTU-in/hr-ft²-°F
@Thickness 0.0118 in
Through Plane; ASTM E 1461
Deflection Temperature at 0.46 MPa (66 psi) 197 °C387 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °FISO 75-1/-2
Glass Transition Temp, Tg 55.0 °C131 °F10°C/min; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
Glow Wire Ignition Temperature  675 °C
@Thickness 0.750 mm
1250 °F
@Thickness 0.0295 in
IEC 60695-2-13
 675 °C
@Thickness 1.50 mm
1250 °F
@Thickness 0.0591 in
IEC 60695-2-13
 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FOptimum, Injection
 260 - 290 °C500 - 554 °FRange, Injection
Mold Temperature 110 °C230 °FOptimum, Injection
 100 - 120 °C212 - 248 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %<= 0.040 %Injection
Hold Pressure >= 60.0 MPa>= 8700 psiInjection
 
Descriptive Properties
AdditivesFlame retardant
Back pressureAs low as possible
Drying RecommendedyesInjection
Max. regrind level (%)15Injection
Part Marking Code>PBT-I-CD40FR(17)<ISO 11469
PolymerPBT FR(17)...
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPBT-I-CD40FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5015n / 254321

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.