MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Old Hickory Wilco-UPF Kaolin Clay
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film strength to ceramic engobes and glazes of all temperature ranges. Wilco UPF also meets the requirements of filler applications where a dry ground processed kaolin can be employed.

Information provided by Old Hickory Clay Company

Key Words: M&M Clays, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.62 g/cc2.62 g/cc
Bulk Density 3.59 g/cc0.130 lb/in³
Moisture Absorption <= 1.00 %<= 1.00 %
Particle Size 0.50 µm0.50 µm32.2% of particles less than
 1.0 µm1.0 µm46.4% of particles less than
 1.3 µm1.3 µmMedian particle diameter
 2.0 µm2.0 µm57.4% of particles less than
 5.0 µm5.0 µm73.3% of particles less than
 10 µm10 µm85.1% of particles less than
 <= 20 µm<= 20 µm91.1% of particles less than
pH 4.5 - 6.54.5 - 6.510% solids
Specific Surface Area 17 m²/g17 m²/g
Brookfield Viscosity 1000 cP1000 cP70% solids dispersed using a Brookfield #3 spindle at 100 rpm
 
Component Elements PropertiesMetricEnglishComments
Al2O3 37.77 %37.77 %
CaO 0.10 %0.10 %
Fe2O3 0.67 %0.67 %
K2O 0.22 %0.22 %
Loss on Ignition(%) 13.18 %13.18 %
MgO 0.050 %0.050 %
Na2O 0.030 %0.030 %
SiO2 45.81 %45.81 %
TiO2 1.74 %1.74 %
 
Descriptive Properties
CEC/MBI (meg/100 ml)3.5
Pyrometric Cone Equivalent (PCE)34
Wet Sieve Residue (%)1Wet Sieve Residue, +325 mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Optigel® WX Clay Additive
Old Hickory Wilco-LPC Kaolin Clay

EOHC926 / 162005

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.