MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic

Material Notes: AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigue, is chemically stable, UV-resistant and has negligible water absorption. It is thermally stable during high temperature processing and post curing without after expansion or outgassing. T90 is designed for easy use with all resin systems and processing technologies. AIREX® T90 is the ideal core material for structural sandwich applications requiring high fire resistance.

Characteristic

  • Good FST Properties (FAR 25.853; NF 16.101; DIN 5510)
  • Excellent fatigue strength
  • Easy to process with all types of resin and lamination processes
  • Excellent long term thermal stability up to 100°C (212°F)
  • Best thermal stability in process up to 150°C (302 °F)
  • High compression strength and modulus
  • Very low variance of the mechanical values
  • Good adhesion (skin-to-core bond)
  • Excellent chemical stability
  • No water absorption
  • No after-expansion, no outgassing
Applications
  • Road and Rail: Floors, sidewalls, font ends, interiors, roofs, engine covers
  • Marine: Decks, interiors, superstructure
  • Industrial: Cover, containers, x-ray tables, sporting good
  • Architecture and Construction: Roofs, claddings, domes, portable building
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.110 g/ccaverage; ISO 845
 0.105 - 0.115 g/cctypical range; ISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1.60 MPain the plane; ISO 527 1-2
 2.20 MPaaverage; in the plane; ISO 527 1-2
Elongation at Break >= 5.0 %shear; ISO 1922
 10 %average; shear; ISO 1922
Tensile Modulus >= 90.0 MPain the plane; ISO 527 1-2
 120 MPaaverage; in the plane; ISO 527 1-2
Compressive Strength >= 1.20 MPaperpendicular to plane; ISO 844
 1.40 MPaaverage; perpendicular to plane; ISO 844
Compressive Modulus >= 75.0 MPaperpendicular to plane; DIN 53421
 85.0 MPaaverage; perpendicular to plane; DIN 53421
Shear Modulus >= 0.0180 GPaASTM C393
 0.0200 GPaaverage; ASTM C393
Shear Strength >= 0.700 MPaISO 1922
 0.800 MPaaverage; ISO 1922
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0330 W/m-KISO 8301

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® T90.150 Easy Processing Structural FST Foam
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam

PZ3AC028 / 108517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.