MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Avient Nymax™ 1200 A UV White 205 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 1.2 %
@Thickness 3.18 mm
1.2 %
@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.018 - 0.024 cm/cm0.018 - 0.024 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.3 MPa10200 psiType I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 79.3 MPa11500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Yield 30 %30 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.96 GPa429 ksiASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 2.90 GPa421 ksiASTM D790
Izod Impact, Notched 0.480 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.899 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded, Across Flow; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
@Thickness 3.18 mm
155 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 60.0 - 107 °C140 - 225 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AdditiveLubricant
 UV Stabilizer
AppearanceWhite
FeaturesGeneral Purpose
 Lubricated
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 LA black (4056) PA6, DAM
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate
Overview of materials for Acetal Copolymer, Unreinforced
Envalior Akulon® K225-KWS Nylon 6 (European and Asian Grade) (Dry)
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)

PH0POL0954 / 145523

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.