MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotch-Weld™ GM15 Gasket Maker Anaerobic Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: 3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal rigid assemblies of any shape or size with high temperature (300°F-400°F) resistance. Additionally, these products fill pits, scratches, and gouges in the flange surface without having to grind or skin the mating surface.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 150000 - 550000 cP150000 - 550000 cPT-bar E @ 5 rpm, Uncured
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 3.45 - 6.89 MPa500 - 1000 psiLap; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -54.0 °C-65.2 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull Cure
 
Descriptive Properties
AppearancePurple

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek M-8 Fiber Seal Pre-cut Gasket
Pyrotek C-1 Fiber Seal Pre-cut Gasket
Process Technologies Inc Viton® Extreme™ Compound 2001 Sanitary Gasket/O-Ring

PMM34694 / 169441

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.