MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Thermx® CG923 NC010 PCT
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced

Material Notes: Thermx® CG923 NC010 is a 20% glass fiber reinforced, flame retardant polycyclohexylenedimethylene terephthalate resin for injection molding.

Celenese acquired the Thermx product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183
Filler Content 20 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527
Elongation at Break 1.8 %ISO 527
Tensile Modulus 8000 MPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 145 MPaISO 178
Flexural Modulus 7200 MPaISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 285 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75-1/-2
UL RTI, Electrical 150 °C
@Thickness 1.50 mm
UL 746B
 150 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 °COptimum
 295 - 310 °C
Mold Temperature 100 °COptimum
 80.0 - 120 °C
Drying Temperature 95.0 °C
Dry Time 4 - 6 hourDehumidified Dryer
Moisture Content <= 0.030 %
 
Descriptive Properties
ColorNatural
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericPCT
Part Marking Code>PCT-GF20FR(17)<ISO 11469
Polymer FamilyPolyester
Polymer TypePCT
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationPCT-GF20FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Crastin® S650FR BK851 PBT-FR(17)
Covestro Makrolon® 6870 Polycarbonate
Cosmic Plastics K77/6220F Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
Celanese Zytel® FR70M30V0 BK010 PA66-MD30FR(17)
Celanese Thermx® CG923 PCT, 20% Glass Reinforced

PDTA7731 / 89690

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.