MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ HSBMR246 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical properties, processability and paintability. It was designed for use in thin-walled bumper fascia applications that require high paint durability. Uses: Automotive exterior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccISO 1183 & ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ISO 868
 70ASTM D2240
Tensile Strength at Break 2470 psiISO 527-1, -2
Tensile Strength, Yield 2800 psiASTM D638
 2900 psiISO 527-1, -2
Elongation at Break 300 %ISO 527-1, -2
 450 %ASTM D638
Elongation at Yield 8.0 %ISO 527-1, -2
Flexural Modulus 210000 psiASTM D790
 218000 psiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -40.0 °C
ISO 180
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Gardner Impact 250 in-lb
@Temperature -30.0 °C
ASTM D3029
Dart Drop, Total Energy 23.0 J
@Temperature -30.0 °C
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
Tear Strength 750 pliASTM D624
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
@Temperature -30.0 - 100 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 203 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 126 °FUnannealed; ISO 75A-1, -2
Shrinkage 0.70 %Tool, 100x150x3.2 mm; Basell Test Method
 0.90 %
@Temperature 121 °C,
Time 3600 sec
Afterbake, 100x150x3.2 mm; Basell Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Adstif EA5073 Polypropylene Copolymer
Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer

PMO799 / 53788

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.