MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
XG Sciences xGnP® Graphene Nanoplatelets
Categories: Carbon; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Pure Graphene Platelets. These are produced in three grades: Grade H, which are platelets with ~15 nanometer thickness (50-80 m2/g) and mean diameters of 5, 15, and 25 microns. Grade M, which are platelets with ~7 nanometer thickness (120-150 m2/g)and mean diameters of 5, 15, and 25 microns. Grade C, which are platelets with thickness less than 2 nanometer, overall diameter less than 2 microns, and are available in surface areas of 150, 300, 500, and 750 m2/g. These materials are furnished as dry black powders (granules) or can be obtained in a dispersion. When used as a filler for polymers, a loading between 3 and 10% is suggested.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/cc
Particle Size 0.0070 µm
Water Vapor Transmission 0.000 g/m²/day
Oxygen Transmission Rate 0.000 cc/m²/day
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 - 100 ohm-cm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aldrich Single Layer Graphene on PET
Goodfellow CVD Graphene Film on Quartz Glass
Goodfellow CVD Graphene Film on Copper Foil
Goodfellow CVD Graphene Film on PET
Goodfellow Ultra Clean CVD Graphene Film on SiO2/Si Wafers

PFLEXBC02 / 179180

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.