MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical GY-SM-30 Plastic Alloy Material Compatilizer Series
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Characteristic:
  • Mixed GY-SM-30 Series with nylon resin, which can enhance the nylon molecular weight during heat reaction and generate chain extension. GY-SM-30 Series can apply on nylon recycling.
  • Add 1-2% GY-SM-30 Series enhance the compatibility with PC/ABS, and can be used as other alloy material compatibilizers, such as compatibilizers, such as PPS/PPO, PA/ABS…..
  • Add 1-5% GY-SM-30 Series can enhance the compatibility of plastic, glass fiber or other inorganic fill and improve the mechanic and surface flatness.
  • Add appropriate amount of GY-SM-30 Series to nonpolarity plastic (such as PP.PE.TPE) can enhance polarity of blend composition. GY-SM-30 Series can apply on print, plating.
  • Add appropriate amount of GY-SM-30 Series to TPE can enhance coverage of polarity material, such as nylon, mental and so on.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 3000 cP
@Temperature 200 °C
3000 cP
@Temperature 392 °F
Melt
Molecular Weight 3800 g/mol3800 g/molNumber-average
 9500 g/mol9500 g/molWeight-average
 
Chemical PropertiesMetricEnglishComments
Acid Value 285285[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 125 °C257 °F
 
Descriptive Properties
Appearancepowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN413 / 266721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.