MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® OM-10265-01 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Appliances; Bonding; Cell Phones; Dental Applications; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Sporting Goods: Toothbrush Handles; Writing Instruments; Soft Touch Application

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62ASTM D2240
 68Aged for 0 hr at 71°F; ASTM D2240
 65
@Time 5.00 sec
Injection Molded, @71°F; ASTM D2240
Tensile Strength at Break 720 psiDie C, 20 in/min, Flow; ASTM D412
 1200 psiDie C, 20 in/min, Across Flow; ASTM D412
Elongation at Break 540 %Die C, 20 in/min, Across Flow; ASTM D412
 780 %Die C, 20 in/min, Flow; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 3.05 mm
All Colors
 HB
@Thickness 6.10 mm
All Colors
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 370 °F
Middle Barrel Temperature 310 - 390 °F
Front Barrel Temperature 310 - 420 °F
Nozzle Temperature 310 - 430 °F
Melt Temperature 330 - 430 °F
Mold Temperature 50.0 - 90.0 °F
Drying Temperature 140 °F
Dry Time 1.00 - 2.00 hour
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceTransparent-Slight Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0899 / 237390

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.