MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Oppera™ PR120 Polymer Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Oppera™ modi?ers are used in packaging for food, confectionery, tea and even cosmetics wrapping, These modifiers are used in the manufacturing of transparent or opaque ?lms with added stiffness and barrier properties. They enable the production of down gauged ?lms, reducing raw material consumption while extending shelf life and product freshness. Altogether, Oppera modifiers support sustainable PP film development.  Benefits: Enhanced optics films with low haze and high gloss, Improved shrinkage, Improved machinability during challenging converting operations, A reduced melt viscosity and the ability to lower stretch/orientation temperatures to reduce power consumption, Possibility for smooth extrusion of difficult polymers with fewer ?lms breaks interrupting operations.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Softening Point 256.3 °FETM 22-24
 
Descriptive Properties
Color (YI)0.2ETM 22-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98956 / 238337

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.