MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-LOY™ Compound A30009 Acrylonitrile Butadiene Styrene (ABS) (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP STAT-LOY A30009 compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing proprietary fillers. Added features of this grade include: Permanently Anti-Static, Flame Retardant.

Features: Flame Retardant,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Moisture Absorption 0.0500 - 0.100 %Injection Molding
Viscosity 12 cP
@Load 5.00 kg,
Temperature 230 °C
MVR cc/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 33.0 MPa5 mm/min; ISO 527
Elongation at Break >= 10 %5 mm/min; ISO 527
Flexural Strength 49.0 MPabreak, 2mm/min; ISO 178
Flexural Modulus 1700 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) >= 55.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+9 - 1.00e+11 ohmASTM D257
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness 1.50 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 195 - 205 °C
Zone 3 205 - 215 °C
Melt Temperature 200 - 210 °CInjection Molding
Mold Temperature 10.0 - 50.0 °C
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81405 / 289352

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.