MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Akulon® S223-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.

Unfilled Extrusion Resins
Akulon resins are available with melt viscosities to suit all extrusion processes: barrier and coating film, tube and hose, monofilament, stock shapes. Akulon resins are characterized by:

  • consistent quality
  • high purity
  • for film applications, low gel contents.

Molding Resins
Suited to all engineering demands:

  • Unfilled low and medium viscosity grades
  • Toughened unfilled grades
  • Glass reinforced from 20-45% filled
  • Low warpage reinforced grades
  • Flame retardant; UL V0 rated and glow wire types
  • Halogen free FR grades
  • Blow moldable materials
  • Laser markable resins
  • Laser weldable, high burst pressure grades
  • Toughened, reinforced resins
  • High stiffness grades for metal replacement

Akulon Ultraflow resins have high flow with mechanical properties similar to standard materials. Exceptional flow allows:

  • productivity gains in molding
  • lower built in stresses
  • better surface appearance
  • system cost reductions

Applications for Molding resins There is an Akulon resin available suitable for any application requiring polyamides. Key areas where DSM has specific application knowledge are

  • Automotive
    • Under the hood and engine components
    • Exterior and interior applications
    • Electrical components and connectors
  • Electrical
    • Low voltage power distribution
    • Lighting
    • Power connectors
  • Consumer Durables
    • Power and lawn and garden tools
    • Small Appliances
    • Sports and leisure equipment
    • Furniture accessories
    • Industrial Goods
    • Transportation (railways)

Information provided by DSM.

Akulon is a former DSM Engineering Plastics product line now with Envalior, although this specific product was discontinued prior to that transaction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc(DAM); ISO 1183
Water Absorption 4.8 %(DAM); Sim. to ISO 62
Moisture Absorption at Equilibrium 1.2 %Humidity Absorption (DAM); Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPaISO 527-1/-2
Elongation at Break 5.0 %ISO 527-1/-2
Tensile Modulus 7.00 GPaISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 10.0 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 4.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C10°C/min (DAM); ISO 11357-1/-3
 
Descriptive Properties
High impact or impact modifiedYes
Injection MoldingYes
LubricantsYes
Release agentYes
With fillersYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 203 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 205 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 207 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Conditioned)
BASF Capron® 8333G Impact Modified, 33% Glass-Filled Nylon 6 (Dry)

PDSMA177 / 31056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.