Availability: North America Forms: Pellets Filler/Reinforcement: Carbon Fiber, 33% Filler by Weight Additive: Molybdenum Disulfide Lubricant Features: Lubricated, Low Friction and Good Wear Resistance Appearance: Black Information provided by TP Composites, Inc. |