MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos ABS Lustran® 1148 General Purpose, High-Impact  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes:

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cmASTM D955
Melt Flow 1.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100
Tensile Strength, Yield 37.0 MPaASTM D638
Tensile Modulus 2.30 GPaASTM D638
Flexural Yield Strength 64.8 MPaASTM D790
Flexural Modulus 2.40 GPaASTM D790
Izod Impact, Notched 4.80 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 92.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 12.7 mm
Unannealed; ASTM D648
Vicat Softening Point 106 °CRate B; ASTM D1525
UL RTI, Electrical 60.0 °C
@Thickness 1.60 mm
UL746B
UL RTI, Mechanical with Impact 60.0 °C
@Thickness 1.60 mm
UL746B
UL RTI, Mechanical without Impact 60.0 °C
@Thickness 1.60 mm
UL746B
Flammability, UL94 HB
@Thickness 1.57 mm
 HB
@Thickness 1.57 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %Opaque only

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Aclo Accucomp ABS ABS802L High Impact Grade
Americhem Engineered Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Ineos ABS Lustran® QE 1094 AS General Purpose, High-Impact

PB1L01 / 26477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.