MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Network Polymers SAN 290 Light Blue Tint
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Description: SAN - Styrene Acrylonitrile Transparent Engineering Thermoplastic

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow  2.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
 8.9 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.9 g/10 min
@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 123123ASTM D785
Tensile Strength, Yield 69.6 MPa10100 psichs 2 in/min; ASTM D638
Flexural Modulus 3.69 GPa535 ksiTangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.160 J/cm0.300 ft-lb/in0.125 inch bar; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C217 °FUnannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 109 °C228 °F0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Optical PropertiesMetricEnglishComments
Haze 2.1 %2.1 %ASTM D1003
Transmission, Visible 86.6 %86.6 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIAM033 / 29871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.