System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical LUSEP FC5400 PPS+GF40%, Injection Molding
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
;
Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Material Notes:
High temperature, Low halogen, Fast cycle time
Application: Automotive, E&E Part
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.60
g/cc
ASTM D792
Linear Mold Shrinkage, Flow
0.0015
cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse
0.0039
cm/cm
@Thickness 2.00 mm
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
190
MPa
@Thickness 3.20 mm
5mm/min; ASTM D638
Tensile Strength, Yield
1940
kg(f)/cm²
Elongation at Break
1.8 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Strength
265
MPa
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus
143000
kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched
7.65
kg-cm/cm
@Thickness 3.20 mm
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+14
ohm-cm
ASTM D257
Dielectric Strength
16.0
kV/mm
@Thickness 1.00 mm
ASTM D149
Thermal Properties
Original Value
Comments
Melting Point
310
°C
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi)
265
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
300
-
320
°C
Middle Barrel Temperature
310
-
330
°C
Front Barrel Temperature
310
-
330
°C
Nozzle Temperature
320
-
340
°C
Melt Temperature
310
-
320
°C
Mold Temperature
120
-
150
°C
Drying Temperature
100
-
120
°C
@Time 14400 - 18000 sec
Moisture Content
0.060 - 0.10 %
Screw Speed
50
-
150
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Celstran® PPS-GF40-01 AD3002 Black PPS, 40% Glass Reinforced
A. Schulman Diamond GPPS BEADS Injection Molding Grade, General Purpose Polystyrene
Precision Polymer Engineering C70C Chloroprene Rubber
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Celanese FORTRON FX4330T7 PPS, 30% Impact Modified
PLHCHEM9824 / 239340
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.