SC 2000-HS is a CNC machined sprayable syntactic polyester used for plug building. MEKP catalyst is not included. Product features: excellent choice for plug manufacturing, offers great vertical hang with no sagging, formulated for very high HDT and low shrinkage. Product benefits: faster plug production turnaround, helps extend life of CNC machine and cutting bits, helps make parts stronger and lighter. Preferred red dye catalyst: HP 90Information provided by ITW Performance Polymers. |