MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M AC-730 Class B-12 Aerospace Sealant
Categories: Polymer; Thermoset

Material Notes: 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on aluminum and between dissimilar metals. 3M AC-730 Class B Sealants have outstanding resistance to aviation gasoline and jet fuel, as well as resistance to chemicals, hydraulic fluids and petroleum products common to the aircraft industry. The mixed compound is a thixotropic paste, easily applied by spatula, extrusion gun or injection gun. They maintain flexibility and bond strength on most metal substrates under extremes of temperature, weathering stress.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³cured 14 days @ 50% RH
Volatiles 2.0 %2.0 %
Brookfield Viscosity 950000 - 1.60e+6 cP950000 - 1.60e+6 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050cured 14 days @ 50% RH
Tensile Strength at Break 2.05 MPa297 psiHeat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C
 2.07 MPa300 psiJRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C
 2.07 MPa300 psiJRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C + Heat Cycle
 2.83 MPa
@Time 1.21e+6 sec
410 psi
@Time 336 hour
Standard cure
 1.86 MPa
@Treatment Temp. 60.0 °C,
Time 1.04e+6 sec
270 psi
@Treatment Temp. 140 °F,
Time 288 hour
JRF
Elongation at Break 60 %60 %JRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C + Heat Cycle
 67 %67 %Heat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C
 525 %525 %JRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C
 460 %
@Time 1.21e+6 sec
460 %
@Time 336 hour
Standard cure
 390 %
@Treatment Temp. 60.0 °C,
Time 1.04e+6 sec
390 %
@Treatment Temp. 140 °F,
Time 288 hour
JRF
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °Fcured 14 days @ 50% RH
 182 °C360 °FShort term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °C-65.2 °Fcured 14 days @ 50% RH
 
Processing PropertiesMetricEnglishComments
Cure Time 7200 min120 hour
Tack-Free Time 6480 min108 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
9.00 Month
@Temperature <=80.1 °F
 
Descriptive Properties
AppearanceBlack
 BlackAccelerator
 Off WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35404 / 170151

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.