MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zoltek™ OX FS 06 X 3 Oxidized PAN Fiber Scrim Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK OX leno pattern scrims are produced from 100% ZOLTEK OX yarns and offer support in applications requiring additional strength and high temperature performance. Also used as the raw material for carbon scrim serving the composite industry. Available plain or with coating. Recommended use: Support in woven & nonwoven fabrics.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.00e+8 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Oxygen Index >= 40 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 62 %
Hydrogen, H 4.5 %
Nitrogen, N 21.5 %
O2 12 %
Sodium, Na <= 0.10 %
Trace Metals <= 0.010 %
 
Descriptive Properties
Areal Weight67.8 g/m2
ColorBlack
ConstructionLeno Weave
Fiber Diameter (µm)12.5
Fill Yarn9/cm
Organic SolventsExcellent resistance
Roll Length45 m.
Roll Width129 cm
Strong AcidsGood resistance
Strong BasesPoor resistance
Warp Yarn15.25/cm
Weak AcidsExcellent resistance
Weak BasesGood resistance
Yarn Input1/10 worsted count

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Pyro-Paint™ 634-CA High Temperature Refractory Coating

ECZO825 / 232296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.