MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® B3 GF 30 FR black (7459) Nylon 6, Glass Fiber, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Flame Retardant Compound. Optimized for small to midsized parts in trains, EN 45545-2. PA 6 GF 25 FR (30+40).

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Filler Content 30 %ISO 1172
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPa5 mm/min. Conditioned; ISO 527-2
 135 MPa5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break 2.7 %5 mm/min. Dry as Molded; ISO 527-2
 6.0 %5 mm/min. Conditioned; ISO 527-2
Tensile Modulus 6500 MPa1 mm/min. Conditioned; ISO 527-2
 10500 MPa1 mm/min. Dry as Molded.; ISO 527-2
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature 23.0 °C
Dry as Molded; ISO 179-1/1eA
 70.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
Dry as Molded; ISO 179-1/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 9.00 kV/mm
@Thickness 1.00 mm
Conditioned; IEC 60243
 9.00 kV/mm
@Thickness 1.00 mm
Dry as Molded; IEC 60243
Comparative Tracking Index >= 600 VDry as Molded. Test solution A.; IEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness 0.800 mm
Conditioned; UL 746A
 >= 120 sec
@Thickness 0.400 mm
Conditioned; UL 746A
 >= 120 sec
@Thickness 1.60 mm
Conditioned; UL 746A
 >= 120 sec
@Thickness 3.20 mm
Conditioned; UL 746A
 >= 120 sec
@Thickness 0.400 mm
Dry as Molded; UL 746A
 >= 120 sec
@Thickness 1.60 mm
Dry as Molded; UL 746A
 >= 120 sec
@Thickness 3.20 mm
Dry as Molded; UL 746A
 >= 120 sec
@Thickness 0.800 mm
Dry as Molded; UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.400 mm
Conditioned; UL 746A
 >= 120 arcs
@Thickness 0.800 mm
Conditioned; UL 746A
 >= 120 arcs
@Thickness 1.60 mm
Conditioned; UL 746A
 >= 120 arcs
@Thickness 3.20 mm
Conditioned; UL 746A
 >= 120 arcs
@Thickness 0.400 mm
Dry as Molded; UL 746A
 >= 120 arcs
@Thickness 0.800 mm
Dry as Molded; UL 746A
 >= 120 arcs
@Thickness 1.60 mm
Dry as Molded; UL 746A
 >= 120 arcs
@Thickness 3.20 mm
Dry as Molded; UL 746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CDry as Molded. DES, 10°C/min; DIN EN 11357-1
UL RTI, Electrical 65.0 °C
@Thickness 0.400 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.800 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 1.60 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 3.20 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.400 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 0.800 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 1.60 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 3.20 mm
Dry as Molded; UL 746 B
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.400 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.800 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 1.60 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 3.20 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.400 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 0.800 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 1.60 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 3.20 mm
Dry as Molded; UL 746 B
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.400 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.800 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 1.60 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 3.20 mm
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.400 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 0.800 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 1.60 mm
Dry as Molded; UL 746 B
 65.0 °C
@Thickness 3.20 mm
Dry as Molded; UL 746 B
Flammability, UL94 V-0
@Thickness 0.800 mm
Conditioned
 V-0
@Thickness 0.400 mm
Conditioned
 V-0
@Thickness 1.60 mm
Conditioned
 V-0
@Thickness 3.20 mm
Conditioned
 V-0
@Thickness 0.400 mm
Dry as Molded
 V-0
@Thickness 1.60 mm
Dry as Molded
 V-0
@Thickness 3.20 mm
Dry as Molded
 V-0
@Thickness 0.800 mm
Dry as Molded
Glow Wire Ignition Temperature 775 °C
@Thickness 3.20 mm
Conditioned; IEC 60695-2-13
 775 °C
@Thickness 3.20 mm
Dry as Molded; IEC 60695-2-13
 800 °C
@Thickness 0.400 mm
Dry as Molded; IEC 60695-2-13
 800 °C
@Thickness 0.800 mm
Dry as Molded; IEC 60695-2-13
 800 °C
@Thickness 1.60 mm
Dry as Molded; IEC 60695-2-13
 800 °C
@Thickness 0.400 mm
Conditioned; IEC 60695-2-13
 800 °C
@Thickness 0.800 mm
Conditioned; IEC 60695-2-13
 800 °C
@Thickness 1.60 mm
Conditioned; IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.400 mm
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 3.20 mm
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 0.400 mm
Dry as Molded; IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
Dry as Molded; IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
Dry as Molded; IEC 60695-2-12
 960 °C
@Thickness 3.20 mm
Dry as Molded; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKRO9932 / 255589

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.