MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
NOVA Chemicals P163B Expandable Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: A fast expanding molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for very low density foam.

Applications: Styrocell P163B is used mainly for producing very low density block. A typical application is drainage boards.

This grade complies with major European and US food contact regulatory regimes, including: European Community Directive 90/128/ECC, including 92/39EEC and 95/EC, relating to plastics materials and articles, intended to come into contact with foodstuffs. Dutch Food Packaging Regulations. Recommendations of German Federal Office of Health (BGA), now regulated by the new Institute of Consumer Health (BGVV), Empfehlung V. US Food and Drug Administration Code of Federal Regulations title 21, sections 177.1640 (Polystyrene) and 178.3010 (Blowing Agents).

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.620 g/cc
Density 0.00900 - 0.0150 g/ccNormal molded density assuming cost optimized selection of processing conditions.
 >= 0.0120 g/ccMinimum achievable; Single stage per-expansion in continuous expander at atmospheric pressure
Bead Size 1.70 - 3.15 mmBerre Laboratory Analytical Methods 0492
 1.70 - 3.20 mm
 
Chemical PropertiesOriginal ValueComments
Styrene Content <= 0.10 %Residual Styrene Monomer Content per Berre Laboratory Analytical Methods 0075
Blowing Agent Content >= 5.9 %Berre Laboratory Analytical Methods 0076

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Overview of materials for Expanded Polystyrene (EPS)
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer

PNOVA332 / 55230

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.