MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.

Elvaloy® 1609 AC is easily processed on standard equipment used for low density polyethylene.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792 - ISO 1183
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238 - ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 97ASTM D2240 - ISO 868
Hardness, Shore D 46ASTM D2240 - ISO 868
Tensile Strength at Break 13.0 MPa500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 740 %500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0800 GPa1 mm/min; ASTM D638 - ISO 527-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 101 °CBy DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 70.0 °CA50 (10N); ASTM D1525 - ISO 306
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 150 °CExtrusion lamination and extrusion coating
 150 °CCast film
 150 °CBlown film
Middle Barrel Temperature 160 °CBlown film
 210 °CCast film
 220 °CExtrusion lamination
Front Barrel Temperature 170 °CBlown film
 250 °CCast film
 290 °CExtrusion lamination
Adapter Temperature 180 °CBlown film
 250 °CCast Film
 290 °CExtrusion lamination
Die Temperature 356 °FBlown film
 482 °FCast film
 554 °FExtrusion lamination
 
Descriptive Properties
MA-Content9 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer
Dow Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Dow Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Dow Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer

PDUPM056 / 33723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.