Hostalen ACP 5331 H is a state of the art HDPE resin, produced by latest Hostalen ACP technology. Hostalen ACP 5331 H is easy processable on injection molding and compression molding equipment. Exceptional organoleptic properties and a good balance of stiffness, toughness and environmental stress cracking resistance make Hostalen ACP 5331 H the choice of customers for the production of closures for sparkling water, CSD and many other types of food and nonfood caps and closures as well as tube shoulders. Applications: Caps & Closures, Collapsible TubesInformation provided by LyondellBasell. |