MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:
  • Excellent stiffness/toughness balance
  • High mechanical strength
  • Very good thermal stability
  • Excellent flammability characteristics
  • Good electrical properties
  • High wear resistance and low friction
  • Very good chemical resistance
  • Good flow and processing properties

APPLICATIONS:

  • Automotive
  • Electrical/Electronic
  • Furniture
  • Construction
  • Home appliances

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183
Filler Content 0.00 %ISO 3451
Moisture Absorption at Equilibrium 2.2 %Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 6.5 %23°C; ISO 62
Linear Mold Shrinkage 0.012 cm/cm
Linear Mold Shrinkage, Transverse 0.012 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527
Tensile Modulus 4.00 GPaISO 527
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 4.00 J/cm²
@Temperature -30.0 °C
ISO 179/eU
 4.50 J/cm²
@Temperature 23.0 °C
ISO 179/eU
Charpy Impact, Notched 0.300 J/cm²
@Temperature -30.0 °C
ISO 179/eA
 0.400 J/cm²
@Temperature 23.0 °C
ISO 179/eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °C10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 230 °CISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CISO 75-1/2
Vicat Softening Point 245 °C50N; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
Glow Wire Test 960 °C
@Thickness 2.00 mm
plaque; IEC 60695

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free
A. Schulman Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0
EMS-Grivory Grilamid® L 20 EC PA12-CD25
EMS-Grivory Grilamid® TR 90 PAMACM12

PEUROT17 / 37247

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.