DELORO® 50 is a hardfacing alloy for application by welding and the Spray-fuse and powder-weld processes and in the form of castings, giving abrasion and corrosion resistant deposits. It is machinable, and has very hard dense corrosion resistant coatings with superior fusing characteristics.Information provided by Kennametal Stellite™ |