MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Fine dust may be irritant. Good chemical resistance. Resistant to termites. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Very Durable (Over 25 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Furniture, interior and exterior joinery. Boat building

Key Words: Tectona grandis; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.550 g/ccGreen, Asian Origin
Density 0.630 g/ccAir Dry (12-15% Moisture Content)
Cell Length 0.700 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2700 NSide
 4100 NSide Hardness, Green, Asian Origin
 4400 NSide Hardness, 12% Moisture, Asian Origin
Tensile Strength, Ultimate 4.10 MPaPerpendicular to Grain
 118 MPaAxial
Modulus of Rupture 0.0800 GPaStatic Bending, Green, Asian Origin
 0.1007 GPaStatic Bending, 12% Moisture, Asian Origin
 0.0790 - 0.131 GPaStatic Bending
Flexural Modulus 11.51 - 13.72 GPaStatic Bending
 9400 MPaStatic Bending, Green, Asian Origin
 10700 MPaStatic Bending, 12% Moisture, Asian Origin
Compressive Strength 41.1 MPaParallel to Grain, Green, Asian Origin
 40.7 - 65.0 MPaParallel to Grain
 58.0 MPaParallel to Grain, 12% Moisture, Asian Origin
Machinability 50 %Medium Relative to Other Wood
Shear Strength 8.80 MPaOrientation Unknown
 8.90 MPaParallel to Grain, Green, Asian Origin
 13.0 MPaParallel to Grain, 12% Moisture, Asian Origin
Impact 5.9J/cm² Toughness
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.60 %Axial; Green to Zero Moisture
 2.5 %Radial Shrinkage Green to Oven Dry, Asian Origin
 3.0 %Radial; Green to Zero Moisture
 5.8 %Tangential; Green to Zero Moisture
 5.8 %Tangential Shrinkage Green to Oven Dry, Asian Origin
 7.0 %Volumetric Shrinkage Green to Oven Dry, Asian Origin
 9.4 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorGolden brown, sometimes with dark markingsUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tropical American Mahogany Wood
African Mahogany Wood
European Ash Wood
American Red Western Cedar (Giant Arborvitae) Wood
Plywood

PTSIH / 71351

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.