Sandvik 6C27 is a martensitic stainless chromium steel with a low carbon content. The grade is characterized by: Soft delivery conditions Excellent formabilityAfter heat treatment the grade has: Good corrosion resistanceHigh toughness Information provided by Sandvik ASTM 420; UNS S42000; EN 1.4028 |