MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Hyosung Topilene R530A PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Product Description: Topilene ® R530A is a specially designed polypropylene random copolymer that features excellent processability and good clarity. It is suitable for pharmaceutical, cosmetic and food contact products. Topilene® R530A complies with FDA requirements in the code of Federal Regulations in 21 CFR 177.1520 for food contact. This product passed the US Pharmacopoeia test(USP class ?) as well as the European Pharmacopoeia test(EP 3.1.6) and can be used as a medical purpose. This product also obtained the Chinese Food and Drug Administration approval and it is registered in the FDA Drug Master File list. (DMF No. 21499)

Typical Applications: Intravenous bottle (EBM) / Cosmetic container / Food container

Features: Excellent processabillity / High transparency

Information provided by Hyosung Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Storage Temperature 40.0 °C104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8080ASTM D785
Tensile Strength, Yield 27.5 MPa3980 psiASTM D638
Flexural Modulus 0.932 GPa135 ksiASTM D790
Izod Impact, Unnotched 0.785 J/cm1.47 ft-lb/inASTM D256
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourair circulated condition
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hyosung Topilene R530 PP

PHYOS67 / 47953

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.