MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Vulkanol® 85 Rubber Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Vulkanol® synthetic plasticizers are required as active ingredients to adjust the properties of vulcanizates, for example, to reduce hardness, modulus and tensile strength or to increase ultimate elongation and resilience. Certain grades contribute to special properties such as improved low temperature flexibility or enhanced green tack of compounds. As a processing aid, plasticizers reduce compound viscosity and improve flow during processing, which results in lower processing temperatures and power consumption.

Key Properties:

  • Improves processing behavior
  • influences important vulcanizate properties
  • contributes to special properties such as low temperature flexibility

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.07 g/cc0.0368 - 0.0387 lb/in³DIN 51 757
Viscosity 40 - 80 cP40 - 80 cPDIN 53019
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.468 - 1.4731.468 - 1.473DIN 51423
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Appearancenearly colorless to yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY9153 / 209544

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.