System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Akulon® Ultraflow K-FHG6 PA6-GF30, Dry, 30% Glass Filled, Heat Stabilized
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Glass Fiber Filled
;
Nylon 6, Heat Stabilized
Material Notes:
30% Glass Reinforced, Heat Stabilized, High Flow
Former DSM Engineering Plastics product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.35
g/cc
ISO 1183
Water Absorption
6.0 %
Sim. ISO 62
Moisture Absorption
1.80 %
Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow
0.0030
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.011
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
160
MPa
ISO 527-1/-2
Elongation at Break
3.0 %
ISO 527-1/-2
Tensile Modulus
9350
MPa
ISO 527-1/-2
Flexural Strength
235
MPa
ISO 178
Flexural Modulus
8500
MPa
ISO 178
Charpy Impact Unnotched
65.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
85.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
14.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+13
ohm-cm
IEC 60250
Dielectric Constant
3.3
@Frequency 1e+6 Hz
IEC 60250
3.5
@Frequency 100 Hz
IEC 60250
Dissipation Factor
0.0050
@Frequency 100 Hz
IEC 60250
0.015
@Frequency 1e+6 Hz
IEC 60250
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
20.0
µm/m-°C
ISO 11359-1/-2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
ISO 11359-1/-2
Melting Point
220
°C
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
ISO 75-1/-2
Flammability, UL94
HB
@Thickness 1.60 mm
IEC 60695-11-10
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Akulon® Ultraflow K-FG6 PA6-GF30, Dry, 30% Glass Filled, High Flow
Envalior Akulon® Ultraflow K-FHG0 PA6-GF50, Conditioned, 50% Glass Filled, Heat Stabilized
Envalior Akulon® Ultraflow K-FHG6 PA6-GF30, Conditioned, 30% Glass Filled, Heat Stabilized
Envalior Akulon® S223-HG6 PA66-GF30, Dry, 30% Glass Filled, Heat Stabilized
Envalior Akulon® Ultraflow K-FG6 PA6-GF30, Conditioned, 30% Glass Filled, High Flow
PDSM8087 / 184788
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.