MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Cast 3135 Low Viscosity Encapsulant
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-CAST 3135 is a low viscosity adhesive developed for demanding electronic underfill and encapsulant adhesive applications. This solvent free material is readily mixed, and cured at room temperature to develop strong bonds to metals, ceramics, glass and many plastics. It can be used in conjunction with TRA-BOND 216D02 to perform `dam` and `fill` functions. Fully cured TRA-CAST 3135 is an excellent electrical insulator and provides resistance to water, gases, acids, alkalis and salt solutions.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/cc
Viscosity 6450 cP
@Temperature 25.0 °C
6450 cP
@Temperature 77.0 °F
Mixed (lv #4, 12 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9292
Adhesive Bond Strength 13.4 MPa1950 psiLap shear, alum to alum, 4 hrs @ 65°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 51.4 µm/m-°C28.6 µin/in-°FBelow Tg
 197 µm/m-°C109 µin/in-°FAbove Tg
Maximum Service Temperature, Air 145 °C293 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 65.0 °C149 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 80 min80 min25 grams
 
Descriptive Properties
Color Black
Mix Ratio, parts by weight100/98Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer

PTRAC108 / 71036

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.