MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® BM73G15P BK317 PA6-IGF15  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced Polyamide 6 Developed for Blow Molding

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccDAM; ISO 1183
Viscosity 350 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
DAM; melt viscosity; ISO 11443
Linear Mold Shrinkage, Flow 0.0040 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 180 MPaDAM; H 961/30; ISO 2039-1
Tensile Strength at Break 70.0 MPa50%RH; ISO 527-1/-2
 110 MPaDAM; ISO 527-1/-2
Elongation at Break 5.0 %DAM; ISO 527-1/-2
 18 %50%RH; ISO 527-1/-2
Tensile Modulus 2600 MPa50%RH; ISO 527-1/-2
 5500 MPaDAM; ISO 527-1/-2
Flexural Modulus 2400 MPa50%RH; ISO 178
 5000 MPaDAM; ISO 178
Poissons Ratio 0.35DAM; ISO 527-1/-2
 0.3850%RH; ISO 527-1/-2
Charpy Impact Unnotched 80.0 kJ/m²DAM; ISO 179/1eU
 110 kJ/m²50%RH; ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²DAM; ISO 179/1eA
 24.0 kJ/m²50%RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 60.0 °CDAM; 10°C/min; ISO 11357-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °COptimum; Extrusion
 235 - 250 °CExtrusion
 260 - 280 °CInjection
 270 °COptimum; Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °CInjection; optimum
Ejection Temperature 210 °CInjection
Drying Temperature 75.0 °CExtrusion
 80.0 °CExtrusion
 80.0 °CInjection
Dry Time 2.00 hourDehumidified; Injection
 4.00 hourDehumidified; Injection
 4.00 hourDehumidified; Extrusion
 6.00 hourDehumidified; Extrusion
Moisture Content 0.050 %Extrusion
 0.20 %Injection
Hold Pressure 50.0 MPaInjection
 100 MPaInjection
 
Descriptive Properties
AdditivesLubricants
 Release agent
Drying Recommendedyes
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time3 s/mm
Max. screw tangential speed0.2 m/sDAM
ProcessingBlow Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Nypel® RC6024 BK 30% Mineral/Glass Filled PA6 (Dry)
DuPont Mobility and Materials Zytel® 70G25HSL NC010 PA66-GF25
Celanese Zytel® ST811HS NC010 PA6-HI
Celanese Zytel® BM73G15THS BK317 PA6-IGF15
Celanese Zytel® 8018HS BKB085 PA66-IGF14

PZDSX5387 / 198027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.